Kynar Flex - PVDF - Arkema

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

A search for "Kynar Flex" in Material Data Center leads to the following information:

Tradename: Kynar Flex
Family: PVDF
Producer: Arkema
30 hits in the material database
1 hits in the literature database


Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.

Kunststoffe international, 2006-06-29, PVDF Foams: High Purity Plus Outstanding Resistance
...ity, and it also has very high flame retardance. On top of this, it is relatively easy to extrude. Using a special foaming process, the firm Zotefoams plc., Croydon/UK, has now succeeded for the first time in producing expanded parts of PVDF (grade: Kynar, manufacturer: Arkema). In this process, extruded sheets of PVDF are exposed to very high pressures at elevated temperature to saturate the material with nitrogen. In a second stage, the sheets expand by being heated in autoclaves under control...


Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.

Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.